Product Notifications
Engineering Change Notification
Public | Finalized Published: 13 December 2005 - Reference: 06_2005_ECN
TAGS: [Mechanical] |
RoHS Surface
Due to the RoHS-directive, Jakob Hatteland Display AS is phasing out the surface treatment currently used on our standard products.
On all the products where we today are using Zinkfosfate or Yellow Chromate, we will in the near future change to the following surface treatment:
Chromital Surtec 650 (Will give a brushed blank surface).
Illustration only

On all the products where we today are using Zinkfosfate or Yellow Chromate, we will in the near future change to the following surface treatment:
Chromital Surtec 650 (Will give a brushed blank surface).
Illustration only

Illustration only
Additional information:
For technical specification see datasheet below. |
Contact:For further enquiries regarding this Engineering Change Notification, please contact Support at Hatteland Technology AS. |
Attachments:
SurTec 650E
(199.5kb) surtec650e.pdf |
Matching products online:
JH 20T03 MMD (HW01)JH 20T03 MIL
JH 17T02 MMD
JH 10T06 MMD
Implemented by:
________________________________
Frode Grindheim
Technical Director
Hatteland Technology AS
Read and Understood by:
________________________________
(Your name)
(Your company)
×